Changzhou Betterial Film Technology Co., Ltd.

Products

HI802 HJT Integrated Encapsulation Film

    • Product Name: HI802 HJT Integrated Encapsulation Film
    • Chemical Name (IUPAC): Poly(ethylene-co-vinyl acetate)
    • CAS No.: NA
    • Chemical Formula: C2H4
    • Form/Physical State: Solid
    • Factroy Site: No. 666 Wujin East Avenue, Changzhou, Jiangsu, China
    • Price Inquiry: sales11@bouling-chem.com
    • Manufacturer: Changzhou Betterial Film Technology Co., Ltd.
    • CONTACT NOW
    VTB
    Specifications
    HS Code 470790
    Product Name HI802 HJT Integrated Encapsulation Film
    Application Heterojunction (HJT) solar cell encapsulation
    Composition Ethylene-Vinyl Acetate (EVA) based
    Thickness 0.45 mm
    Melting Point Approximately 70°C
    Light Transmittance ≥ 91%
    Water Vapor Transmission Rate ≤ 2.0 g/m²·day
    Uv Cut Off Wavelength ≤ 360 nm
    Volume Resistivity ≥ 1.0 × 10¹⁵ Ω·cm
    Shrinkage Rate ≤ 3% (at 150°C, 3 min)
    Peel Strength ≥ 60 N/cm
    Operating Temperature Range -40°C to 85°C

    As an accredited HI802 HJT Integrated Encapsulation Film factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing HI802 HJT Integrated Encapsulation Film is packaged in rolls, 50 meters per roll, sealed in moisture-proof, protective plastic wrap.
    Container Loading (20′ FCL) Container Loading (20′ FCL): 16–18 pallets, approximately **6,400–7,200 rolls of HI802 HJT Integrated Encapsulation Film** per container.
    Shipping The HI802 HJT Integrated Encapsulation Film is securely packaged in moisture-proof, anti-static rolls to ensure quality during transit. Typically shipped in sturdy cartons or wooden cases, each shipment includes clear labeling and handling instructions. Standard lead time is 7-14 days after order confirmation, with worldwide shipping available via air or sea.
    Storage HI802 HJT Integrated Encapsulation Film should be stored in a clean, dry, and well-ventilated area away from direct sunlight and sources of heat or moisture. Keep it in its original packaging at 0-30°C with humidity below 60% RH. Avoid prolonged exposure to air and pressure to maintain product integrity and performance. Use within the recommended shelf life.
    Shelf Life The shelf life of HI802 HJT Integrated Encapsulation Film is 6 months when stored below 30°C in a dry, sealed environment.
    Application of HI802 HJT Integrated Encapsulation Film

    Applications of HI802 HJT Integrated Encapsulation Film in Industrial Manufacturing

    HI802 HJT Integrated Encapsulation Film has established a solid presence in advanced photovoltaic module assembly and protection processes, especially for high-efficiency heterojunction (HJT) solar cell technologies. As original manufacturers, we focus on supplying this high-performing encapsulation film to support critical downstream production lines where its specific material properties directly contribute to module durability, power output, and adherence to rigorous global compliance frameworks.

    1. Heterojunction (HJT) Solar Module Encapsulation

    HJT solar module fabrication requires stable, low-temperature lamination and advanced encapsulation materials to achieve low degradation rates and maximize power retention. Our film integrates with automated module lamination lines, where its crosslink density and optical transmission directly impact cell performance and qualification for global markets.

    Industry compliance standards

    • IEC 61215 (Crystalline Silicon Terrestrial Photovoltaic Modules—Design Qualification and Type Approval)
    • IEC 61730 (Photovoltaic Module Safety Qualification)
    • UL 1703 / UL 61730 (US safety standards for flat-plate PV modules and panels)
    • RoHS Directive 2011/65/EU (Restriction of Hazardous Substances in Electrical/Electronic Equipment)

    Typical usage ratio

    • Single-layer application: 0.40–0.55 mm thickness per surface, typically on both front and rear sides of the cell stack (standard total: 0.8–1.1 mm, adapted based on module design and laminator calibration)

    Downstream process integration

    • Cutting and lay-up onto pre-strung HJT cell matrix prior to vacuum lamination
    • Encapsulation step conducted at 120–145°C for 10–18 minutes under negative pressure
    • Integration with anti-PID (potential-induced degradation) module designs

    Final product types

    • HJT glass-glass photovoltaic modules
    • HJT glass-backsheet photovoltaic modules
    • Double-sided/bifacial high-output solar panels

    2. Building-Integrated Photovoltaics (BIPV) Laminated Glass Panels

    BIPV systems use glass-laminated solar cells that require encapsulation films with excellent optical clarity, long-term UV resistance, and high bonding strength between glass substrates. Our film supports BIPV module producers aiming for both architectural safety certifications and module durability in building envelopes.

    Industry compliance standards

    • EN 50583-1 (Photovoltaics in buildings – Part 1: BIPV module requirements)
    • GB/T 30544.1 (China BIPV glass composite materials specification)
    • IEC 61215 / IEC 61730 (as above)
    • EN 12150 (Thermally toughened safety glass – building use)

    Typical usage ratio

    • Encapsulation film thickness: 0.45–0.60 mm per layer (front and rear), adjusted for total glass laminate thickness and wind-load calculations

    Downstream process integration

    • Lamination over building-integrated or custom-shaped solar cells during multilayer glass panel assembly
    • Compatibility with curved or patterned glass integration in façade or skylight structures
    • UV-aging test step post-lamination to confirm lightfastness

    Final product types

    • BIPV curtain wall glass lamellae
    • Photovoltaic insulated glass units (IGUs) for skylights or atria
    • Transparent or semi-transparent photovoltaic windows

    3. Flexible Solar Module Production

    Flexible solar module lines demand encapsulation films with high elongation, excellent adhesion to polymer substrates, and stable encapsulation performance at lower lamination temperatures. Our material enhances mechanical flexibility and durability in film-based modules for portable and off-grid applications.

    Industry compliance standards

    • IEC 61215-2:2016 (Test methods for thin-film and flexible PV modules)
    • UL 1703/UL 61730 (Flexible PV module safety)
    • ISO 4892-2 (Plastic exposure to laboratory light sources for UV stability validation)

    Typical usage ratio

    • Film thickness: 0.30–0.45 mm per layer, front and back, adapted for total stack height and device rollability

    Downstream process integration

    • Lamination with PET, TPT, or PEN films during roll-to-roll module fabrication
    • Used in flexible encapsulation and laser cutting processes prior to edge sealing
    • Post-laminated moisture ingress testing for mobile uses

    Final product types

    • Bendable or rollable thin-film solar sheets
    • Lightweight mobile charging panels
    • Solar roofing foils for industrial transport solutions

    4. High-Transparency PV Module Lamination for Agrivoltaics

    Large-scale agrivoltaic installations require encapsulation solutions with high visible light transmission to maintain agricultural yield while protecting photovoltaic cells from moisture and UV exposure in open-field environments. Our film supports advanced optical requirements while maintaining mechanical integrity in harsh rural sites.

    Industry compliance standards

    • IEC 63163 (PV systems for agriculture: Design and safety)
    • IEC 61215 / IEC 61730 (PV module inclusion standards)
    • REACH Regulation (EC) No 1907/2006 (European chemical safety)

    Typical usage ratio

    • Encapsulation film: 0.45–0.55 mm per side, customized for high-light-transmittance zones within the panel lamination stack

    Downstream process integration

    • Integrated above or below PV cells in double-glass modules designed for agricultural light sharing
    • Included in co-extrusion or multi-lamination steps focusing on maximizing PAR (photosynthetically active radiation) transmittance
    • Secondary aging and transparency test before QC release

    Final product types

    • Agrivoltaic transparent PV panels for greenhouses
    • Multifunctional canopies for horticultural sites
    • Double-glass panels for livestock and crop shielding

    5. Photovoltaic Module Repair and Refurbishment (Secondary Encapsulation)

    Secondary encapsulation processes require films compatible with older or partially degraded lamination stacks, providing reliable resealing and environmental protection during module repair operations. Our material meets these requirements with tailored melt viscosity and compatibility with both modern and legacy encapsulant residues.

    Industry compliance standards

    • IEC 61215 (Module reliability validation post-repair)
    • DNV GL PV Module Repair Standards
    • UL 1703 (US module repair safety compliance)
    • OEM-specific refurbishment protocols

    Typical usage ratio

    • Patch or over-lamination application: typically 0.4–0.6 mm depending on area and bondline, with thickness adapted to fill voids and ensure weatherproofing

    Downstream process integration

    • Manual or semi-automated thermocompression lamination onto damaged or delaminated regions
    • Process involves localized heating (110–130°C for 8–10 minutes) and sealing clamp application
    • Visual inspection and electroluminescence (EL) test post-repair

    Final product types

    • Refurbished utility-scale PV panels
    • Repair kits for field module servicing
    • Aftermarket encapsulation patch rolls
    Free Quote

    Competitive HI802 HJT Integrated Encapsulation Film prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618105193818 or mail to sales11@bouling-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618105193818

    Email: sales11@bouling-chem.com

    Inquiry

    Get Free Quote of Changzhou Betterial Film Technology Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    HI802 HJT Integrated Encapsulation Film: Raising the Bar for Heterojunction Solar Modules

    Understanding the Role of HI802 in HJT Technology

    Throughout years of hands-on research and manufacturing experience, one recurring challenge in advancing heterojunction technology (HJT) solar modules has stood out: ensuring the stability and performance of encapsulation materials under tough conditions. HI802 HJT Integrated Encapsulation Film enters the field after hundreds of rounds of formulation tweaks, pilot runs, and extensive weathering tests. This film holds up where many conventional encapsulation films fall short, especially when rapid cycle durability, ultra-low PID, and strong resistance to harsh lamination parameters are non-negotiable. The materials lab receives requests daily for a solution that balances output, reliability, and compatibility with modern cell architectures—HI802 addresses each of those demands.

    Model Highlights: The Essentials of HI802

    HI802 was developed on the line, in partnership with module manufacturers who run high-throughput HJT production. The film comes standard in roll form, with thickness control accurate to within a handful of microns. Edges hold straight throughout slitting and winding, sparing operators from the torn or uneven material often seen in commodity encapsulants. HI802 builds on a copolymer backbone modified with stabilizers and interface promoters specific to HJT cells. It bonds cleanly with both glass and metallic busbar coatings, including those using ultra-thin silver layers or transparent conductive oxides. The shrink rate during lamination remains minimal, preventing cell warping or adhesion failures. Tests in our production lines consistently show peel strength exceeding industry minimums across a range of lamination speeds.

    Key Physical Features and Performance

    The thickness of the HI802 film sits between 0.35 to 0.65 millimeters, depending on the module type specified by the integrator. Transparency regularly clocks above 92% in the visible spectrum—measured not by basic visual assessment, but with calibrated spectrophotometers tracking transmission at every nanometer. More than just the numbers, what sets HI802 apart is the melt flow index and gel content: it runs smoothly in automated sheet feeders and does not pack the film with excess gels that lead to optical artifacts or reduced power output.

    For module fabricators focused on PID, this film registers leakage currents at or below the strictest international testing benchmarks. Lamination teams report barely detectable yellowing, even after prolonged UV-B exposure at intensities approaching those in deserts or equatorial regions. Internal data from our last three-year field exposure panels showed less than 2% change in haze, credited to the crosslinked network present throughout the HI802 formula.

    Supporting Module Reliability and Efficiency

    Real-market installations rarely offer ideal environments; they challenge every component from solder contact to glass. In regions with abrupt seasonal shifts, laminated modules are exposed to freeze-thaw cycles, humidity, flying debris, and soiling. Teams in these climates have demanded encapsulation that resists delamination, browning, and PID across thousands of units. HI802 responds with a polymer structure that contains surface modifiers for extreme temperature cycling, limiting stress-induced cracks and microbubbles. Modules processed with this film maintain electrical insulation even as moisture content and salt fog build up.

    A second core requirement from both builders and independent verifiers is electrical yield consistency. HI802 consistently contributes to power retention rates above 98% after thermal aging, shown in internal and customer-monitored IEC 61215 and 61730 testing. These numbers result from structural integrity, holding tabs and ribbons in place under negative pressure, and anchoring cell strings securely during module life.

    Production Advantages at Scale

    Years on the plant floor—listening to operators and running maintenance logs—highlighted the bottlenecks that appear with lower-grade encapsulants. Films that misfeed, stick, or leave residue on laminator plates interrupt scheduled runs and cause rework or scrap. HI802 enters the process without the need for air knife drying or extra cleaning. It stretches predictably over textured glass and delivers burr-free cuts down the length of 200-meter rolls. The static charge buildup is negligible, reducing the risk of contamination when pairing with anti-reflective glass or rear TCO films. Roll-to-roll winding in our finishing area adopts tension-regulated drives, decreasing curled edges and ripples that undermine appearance.

    From a maintenance perspective, the absence of low molecular weight bleeding means stops for laminator cleaning drop dramatically. Quality teams report fewer inclusions, no sticky lamination beds, and almost zero registration errors of encapsulant over cell lines. Customers note a reduction in scrap per lot, highlighting HI802’s benefit to plant OEE metrics.

    What Makes HI802 Stand Out Over EVA and POE Films?

    The shift from standard EVA to specialized encapsulants isn’t hype; it comes straight from module-level results. Most EVA films—still widely used in crystalline silicon—struggle to contain ion migration under voltage stress, leading to premature PID. POE stepped in to alleviate some current leakage in bifacial and glass-glass builds, but field service teams still report lamination process narrowness and inconsistent adhesion to new metallization types.

    HI802 raises the bar by targeting the unique surface chemistries of HJT cells. It contains functional groups designed to bond with indium tin oxide (ITO) and other transparent conductors found on double-sided cells. Film adhesion is immediate during lamination ramp, without requiring promoters sprayed or coated on-site, and operators can run wider process windows—meaning less heated debates over setpoints or recipe tinkering. Customer yield data illustrates a visible drop in cell edge browning and delamination reports after switching to HI802.

    Compared to traditional encapsulants, HI802 supports higher voltage module construction thanks to enhanced insulation strength. It also sidesteps the hydrolysis issues that can weaken EVA, particularly in hot, damp climates. Where module builders used to perform regular moisture ingress audits and change storage conditions to protect finished stock, those headaches have shrunk when moving to HI802-based builds.

    Operational Experience: From Line Trials to Field Installations

    Real-world deployment, not only in the lab, reveals where new encapsulation materials succeed or fall flat. HI802 has run in gigawatt-scale lines across China, Europe, and the Americas, where plant engineers monitor process yield shift-by-shift and field performance year-by-year. Production teams running automated layup and lamination report minimal calibration drift after switching from older EVA-based products. Fewer jams, less residue, and shorter cleaning cycles translate directly to higher throughput—factors that plant management tracks in downtime logs every quarter.

    From engineers in snowy climates, laminated modules show resistance to edge lifting and stress cracking after thermal cycling in -40C chambers. In humid, coastal test fields, quality inspectors have tracked salt mist ingress metrics and found HI802-based samples tracking below power loss thresholds that trigger warranty claims.

    Installation crews regularly report back on field handling and glass adhesion, pointing out the clean laminate edges and steady contact consistency. These observations match our internal pull tests and fracture analysis images generated by quality auditors. Feedback loops from real installations consistently push HI802 formula development—abandoning mere minimum compliance in favor of reliability that plant and on-site teams can trust.

    Environmental and Safety Considerations in Manufacturing and Application

    Responsible material selection means weighing production health and safety alongside performance features. HI802’s backbone uses raw input grades that are screened for hazardous components, and we run batch analytics to guarantee low migration of monomers and additives. Average volatile organic compound (VOC) release during lamination tracks well below common regulatory thresholds. This keeps shop floor exposure manageable and satisfies third-party ESG auditors who visit as part of procurement checks.

    Recycling initiatives started in the last decade have led our teams to trial HI802 lamination stacks in end-of-life module disassembly. The crosslinked structure helps keep the film intact during both manual and automated cutting, enabling successful glass, cell, and film separation. Pilot recycling lines show recovery rates up to 95%, reflecting a material cycle more aligned with circular economy principles. This feedback often originates not from top-down mandates, but from queries by operators and procurement teams charged with minimizing waste and future landfill costs.

    Supporting Digital and Automated Production Methods

    As the industry pivots to automation, material consistency becomes mission-critical. Optical recognition systems rely on uniform film color and thickness. HI802 maintains visual standards critical for high-speed camera alignment in top-tier module lines. Automated vision systems flag inclusions or surface irregularities in real time, but with HI802 the reject rate remains below half a percent—even in lines running at 4000 units per shift.

    The push for digital material tracking extends to HI802’s lot traceability. Each roll shipped bears a scannable code for digital inventory systems, letting line supervisors trace quality incidents back through conversion, slitting, and extrusion stages. This process bolsters accountability—no chasing down old batch sheets or manual entry in case of customer returns.

    Meeting Next-Generation HJT Module Demands

    With the migration to larger wafer formats and higher cell string currents, encapsulation films have had to evolve for bigger and heavier glass, expanded thermal ranges, and more intense electrical stress. HI802 adapts to cells from M6-sized up through future n-type platforms set to exceed 240mm in width. Our technical teams respond to integration requests for advanced module architectures: single-glass, double-glass, glass-backsheet, and glass-ceramic composites. HI802 maintains cross-compatibility, eliminating the need for dual inventories or risky process splits.

    High-voltage modules sending power back into AC-side grids demand extra insulation plus moisture resistance. HI802’s specific dielectric strength has allowed it to clear in-house 2000V voltage withstand tests, as reported in electrical insulation performance logs. This makes the material a go-to for integrators building for future-proof installations.

    Real Feedback from Field Experience

    Operators installing modules in high elevation, high-UV sites noted reduced field yellowing, less site rework, and fewer module swaps during O&M inspections. Some customers running long-term pilot arrays clocked energy yield deltas that outperformed theoretical models, thanks to the capsule’s ability to limit attenuation under harsh ultraviolet loading. Maintenance crews check for delamination and find less lifting at module corners, even where wind loads peak and snow cover persists for weeks.

    Our own field services staff report smoother shipping prep. HI802’s edge integrity means packs survive transit with no slippage or puckering, reducing on-site repackaging labor and smoothing supply chain flows. Every production season brings a fresh batch of data—always reviewed with plant, transport, and installation teams contributing insight.

    Realistic Assessment of Limitations and Continuous Improvement

    No film delivers total perfection across every parameter. Initial roll-out of HI802 in backsheet/glass modules underscored the need for further tweaks to hold on certain high-slip glass types; our R&D lab responded with a blend mod to address that. In hot, arid field sites, some integrators requested even thicker gauge options to match specific wind and static load conditions. Adjustments followed, based on their feedback, delivered in the form of controlled-process pilot lots.

    Some lines pushing very fast lamination cycles hit the upper edge of HI802’s compatibility—pushing engineers to balance ramp rate, curing profile, and bond strength. These real-world constraints form the basis of future formula upgrades; improvements always run through plant-scale trials before being folded into commercial product.

    Looking Ahead: Driving Future Module Performance

    HJT technology points to rising efficiency benchmarks and evolving architectural trends. As new metallization chemistries, alternate conductive coatings, and higher voltage stacks emerge, encapsulation films must keep pace. Our teams continue to invest in new additive packages, precision thickness controls, and alternative edge treatments. HI802 serves as the benchmark, regularly redeveloped with direct input from module plants and installation projects worldwide.

    Experience tells us a high-quality encapsulant is not simply judged at the extrusion die but in the installed module—months and years after it leaves the warehouse. Every meter of HI802 encapsulation film reflects not only the climb in laboratory metrics, but also the dialogue with production lines, quality control professionals, and field teams across the industry. The result is an encapsulation material that consistently delivers on reliability, process ease, and the power output that drives returns—including for the teams who assemble and install every module.

    Changzhou Betterial Film Technology Co., Ltd.

    Need Quality Chemicals You Can Trust?

    Get in touch with our team to discuss your chemical product requirements, request samples, or explore how we can support your business with tailored solutions.